Moisture Testing and Moisture Surveys: Assessing Concrete Floors for Coating Readiness

From JPCL, August 2016

By Brian O’Farrell, DP Coatings Ltd.

There are many ways moisture can affect concrete floor coatings but moisture testing alone is not sufficient to detect all potential problems. Sometimes problems are not apparent or may not even exist until coatings have been applied. Performing a moisture survey — an inspection of a building and its environment prior to performing any tests — will provide a clearer picture of the potential problems moisture in both liquid and vapor form can pose....


(Login to read the full article)
   

Tagged categories: Coating failure; concrete; Concrete floor coatings; Humidity and moisture; Surface preparation; Surface Preparation; Testing + Evaluation

Comment from Furqan Muhammad, (9/22/2016, 2:30 AM)

gOOD Moorning I Appriciate this articles.its value assets for me. Regards Muhammad Furqan Coating Inspector Protective,Marine and Offshore Coating


Comment from Michael Quaranta, (9/23/2016, 1:41 PM)

Say Brian, Grest article but you opened questions. Can you list the seven (7) changes that have been made and adopted by the consensus process in the ASTM Committee? The ASTM F-1869 started in 1998 with some serious questions and in 2002 the ACCA issued a rejection of the entire supposed test. How about you and i get together to straighten out this "moisture" determination solved with more quantum physics truth than consensus opinion?


Comment Join the Conversation:

Sign in to our community to add your comments.

 
 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us