Experts Weigh in on Bay Bridge Cable

Wednesday, October 14, 2015

Comment | More

Concerns about corrosion on the San Francisco-Oakland Bay Bridge have prompted a team of bridge professionals to ask for quick action to protect the main cable supporting the bridge.

After last week’s reports that the project’s lead designer feared rainwater exposure would lead to corrosion of the main cable, a panel of bridge maintenance experts have stepped forward to state that an “immediate retrofit” is in order, SFGate reported Tuesday (Oct. 13).

Photos: Caltrans

The Bay Bridge oversight committee and Caltrans have enlisted a panel of experts to contribute their analysis and input on the structure over the course of a year.

The Bay Bridge oversight committee and Caltrans had enlisted this panel of experts to contribute their analysis and input on the structure over the course of a year. It is this same team who reported on the corrosion of the tower rods as well.

Their attention is now on the integrity of the main cable, as well as maintenance access on the structure.

Expert Analysis

Made up of officials from the Golden Gate Bridge, the Bronx Whitestone Bridge, Hong Kong’s Tsing Ma Bridge and Scotland’s Forth Road Bridge, the experts point to corrosion that has occurred on bridges with similar cable structures to support their concerns.

“Cracks in wires and wire breaks have been found within the cables of a significant number of suspension bridges,” according to the panel.

“It would appear that there is now serious doubt on whether the traditional method of painting to provide protection to the main cables of these bridges is sufficient to provide a service life similar to the full design service life of the bridge.”

The experts suggest that the “conventional method” of utilizing corrosion-fighting coatings, applying a protective layer of paint and enclosing it in a steel jacket may not be effective on its own.

Other protection options include dispensing a corrosion-fighting oil into the enclosed cable or blowing air inside the cable.

The first approach would require the existing cable to be opened up along “much of its length” and is an expensive option, the panel says. The second is becoming a more popular method on new bridges.

What’s Next?

According to reports, Caltrans had considered installing a system to blow air at a low pressure into the cable but decided it was too new and untested.

Reports indicate the cost for installing a dehumidification system would run in the tens of millions of dollars.

However, the maintenance experts say they are certain such a method would work and that it’s not too late to employ the air system.

“Unless there are overwhelming difficulties that prevent such a system from being fitted, it should be installed as soon as possible,” their report said.

The chair of the Bay Bridge oversight committee, Steve Heminger, indicated this dehumidification method would be discussed with Caltrans.

“Corrosion and cracking is what you look for on every bridge, not just the Bay Bridge,” Caltrans said in a statement reported by SFGate. “We are employing some dehumidification, and if more is warranted we will address that.”

Reports indicate the cost for such an installation would run in the tens of millions of dollars. Bay Bridge officials have access to a pool of maintenance money available to state-owned toll bridges, but here, too, the toll-payers are likely to absorb some portion of the cost.

Maintenance and Prevention

Of additional concern to the maintenance panel, the structural design itself is likely to hamper inspection and maintenance efforts. “Many crucial areas are all but inaccessible,” according to SFGate.

The following areas have been cited in the experts’ report:

  • Because the main cable and smaller supporting cables pass over a busy roadway, repair work poses a risk to both workers and drivers.
  • Inspectors are unable to get inside the steel-encased main cable to look for corrosion.
  • The cable ends are housed inside anchorages within the deck, rather than above the bridge surface. The group said this transfers “extremely high compressive forces into he deck” that not only make maintenance difficult but also could lead to cracking of the concrete support piers.
  • Beneath the road deck, it is impossible to check the steel tendons that hold the Skyway portion of the bridge together.

Caltrans doesn’t argue the difficulties posed by the bridge design. “It’s no secret that there are access challenges to this bridge,” it said in its statement. “That won’t stop us from protecting it. We’re open to considering any suggestion in the report.”

   

Tagged categories: Asia Pacific; Bridge Piles; Bridges; Corrosion; Corrosion protection; Dehumidification; EMEA (Europe, Middle East and Africa); Latin America; North America; Quality Control

Comment from Fred Wittenberg, (10/14/2015, 7:14 PM)

It just got an award, but the hits keep on coming, as I told my wife as we crossed it to & fro SF. As an engineer, it just overwhelms me that ease of bridge maintenance literally fell into the bay.


Comment from Randy Gordon, (10/14/2015, 10:08 PM)

I like the may or might fear tactic. We opened up the casing on the SFOBB cables during the retrofit in 2001-2004 and the lead paste that covered all of the cable strands was pristine from 1937. Smeared more lead paste into it and put it back together. Robert ikenberry...remember? Lead...Best barrier ever and still performing after 80+ years.


Comment from Robert Ikenberry, (10/16/2015, 11:25 PM)

Yes Randy, I remember! Good old red lead paste was the "gold standard" for corrosion protection for a long, long time - for good reason.


Comment from Tom Schwerdt, (10/22/2015, 4:26 PM)

Can't beat red lead for cost effective long-term corrosion protection of steel in many environments...


Comment Join the Conversation:

Sign in to our community to add your comments.


 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us