Coatings Industry News

Main News Page


New Standard Addresses H2S Corrosion

Monday, August 1, 2016

Comment | More

The British Standards Institution (BSI) has issued a new standard for testing a common and dangerous type of corrosion and cracking in oil and gas pipelines.

The new document, BS 8701: Full Ring Ovalization Test for Determining the Susceptibility to Cracking of Linepipe Steels in Sour Service—Test Method, covers cracking problems in steel pipelines, caused by the presence of wet hydrogen sulfide (H2S).

Sour Service

Environments that contain H2S are considered to be “sour,” as opposed to “sweet.” When sour corrosion takes place, iron sulfides are formed on the corroded surface. This then leads to hydrogen accumulation, which is eyed as a cause of pipeline cracking.

Sulfidic corrosion was blamed for the August 2012 leak and subsequent fire at Chevron’s Richmond, CA, refinery.

Corroded pipe at Richmond refinery
Anamet Inc.

Sulfidic corrosion was blamed for the August 2012 leak and subsequent fire at Chevron’s Richmond, CA, refinery; a corroded pipe from that facility is pictured here.

The new standard updates the U.K.’s Health and Safety Executive’s guidance document OTI 95 635, addressing the same topic, published in 1996. According to BSI, the previous standard was not up to date with regard to sour service lines.

Ring Specimen Test

According to BSI, the standard discusses assessing a pipeline’s susceptibility to cracking by testing a ring specimen “where a stress level is applied to two regions of the specimen” and a sour test solution is applied. The specimen is monitored and studied to determine whether cracking begins or expands.

While sour corrosion is also known to take place in wastewater pipelines, the new standard from BSI is tailored to the oil and gas industry, and was authored with the help of industry experts, the organization says.

“Having a test method such as BS 8701 in place allows the correct tests for identifying the damaging levels of corrosive hydrogen sulfide gas, to be carried out,” said David Fatscher, Head of Market Development for Sustainability and Energy at BSI. “It can act as an early warning system that offers reassurance that everything is being done to safeguard the environment.”

The standard can be purchased here.

   

Tagged categories: Asia Pacific; Certifications and standards; Corrosion; Cracking; EMEA (Europe, Middle East and Africa); Latin America; North America; Performance testing; Pipeline; Quality Control; Steel

Comment from Krishnan Swaminathan, (8/1/2016, 9:23 AM)

As told it is a very dangerous and a catastrophic form of corrosion which may at times lead to sudden material failures. The standard introduced is a must and we have to study the same before commenting on its efficacy which may be expected to be good.


Comment Join the Conversation:

Sign in to our community to add your comments.


 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us