Abnormally dry conditions in one southern state appear not only to be putting restrictions on residents’ recreational activities, but also taking a toll on state highways.

“Our roads have suffered the effects of extreme loss of rainfall throughout Mississippi,” Mississippi Department of Transportation Commissioner Tom King, Southern Transportation District, said in a statement.

“Our biggest problem is large cracks in the asphalt that are becoming a hazard for the traveling public,” he added, although state officials are not aware of any accidents having occurred as a result of the cracked road surfaces.

Hwy 41 cracking
Photos: Mississippi Department of Transportation

The drought in Mississippi this year is not only affecting recreational activities such as bonfires and camping, but it’s also affecting the state’s highways, according to the Mississippi Department of Transportation. “Our biggest problem is large cracks in the asphalt that are becoming a hazard for the traveling public,” said MDOT Commissioner Tom King.

The problem is affecting roads statewide, even newly paved portions of Highway 463, station WDAM reported.

“It’s not unique to one part of the state,” MDOT spokesman Jason Scott told the Sun Herald, which serves southern Mississippi.

"I just caution people be careful, watch out," Commissioner Dick Hall, Central District and chair of the Mississippi Transportation Commission, told WDAM.

"We know it's there, we're trying to spot them as fast as we can and put some kind of warning out there and try to fix them as fast as we can."

Clay Subsurface

According to MDOT, the crumbling roads are resulting from the impact of extreme drought conditions on the soils beneath the roadways.

Mississippi has large deposits of at least three different types of expansive clay soils, including Yazoo clay, throughout the state.

These soils pose a challenge for road construction and maintenance because they are susceptible to change based on weather conditions, the agency says.

Yazoo clay, for example, can expand and occupy up to 400 percent more space when wet than at normal moisture levels—but, as the soil loses moisture, it shrinks, leaving a void between the soil and asphalt or layer of earth above it.

As soil continues to shrink, the void becomes larger and the weight of the pavement and vehicles causes the roadway to sink and crack creating “slides” and “drop offs,” MDOT explains.

Hwy 49 cracking

MDOT says at least three different types of expansive clays in the state’s soils pose a challenge during road construction and maintenance because of how they change with weather conditions, such as expanding greatly when wet, then shrinking and leaving voids behind in dry conditions.

“When traffic goes over it multiple times, that’s what creates the cracks,” Scott told the Sun Herald.

However, Scott notes, repairs aren't going to be as simple as an overlay; rather, damaged sections will reportedly need to be dug up for soil to be to replaced underneath.

When the drought ends, MDOT says it will assess the overall needs and extent of the damage before any roads are properly repaired.

Trees and Pavement

Rural highways lined with trees are suffering the most from cracking asphalt, transportation officials add.

This is because in the mid-1900s county roads given to the state resulted in a paved network of farm-to-market routes—many of which are today’s Mississippi highways. This translates to a narrow right-of-way lined by trees.

“As the trees reach further for water during extreme drought, the close proximity of trees to the roadway combined with expansive clay soils accelerate the shrinkage of the underlying roadbed materials,” says MDOT Executive Director Melinda McGrath.

When fully grown, a tree will absorb 100 gallons or more of water from the ground on a hot day, the agency explains. So, during drought conditions, trees located close to the road draw all the moisture out of the soil beneath the roadbed.

This, coupled with already shrinking soil, will cause major damage to the highway, MDOT says.

Hwy 245 cracking

When the drought ends, MDOT will assess the overall needs and extent of the damage before any roads are properly repaired. "We already know it will take more than simply placing a lift of asphalt to repair most highways," said MDOT Executive Director Melinda McGrath.

"With limited resources, it’s not an option to obtain more right-of-way along state-maintained highways to minimize the effects on existing routes,” McGrath notes.

Anticipating Repairs

MDOT reporteldy accounts for later extreme weather conditions during the design phase of a project.

"We already know it will take more than simply placing a lift of asphalt to repair most highways," McGrath says.

"Severe weather events such as droughts and ice storms prematurely age pavements, forcing MDOT to alter the three-year paving schedule to repair damages," she explains.

Current strategies MDOT employs for extreme weather conditions include:

  • Specifying embankment materials that limit the amount of clay;
  • Undercutting and replacing problematic clay material just beneath the pavement structure;
  • Treating the soil at the bottom of the pavement structure with lime or cement;
  • Providing wide shoulders to support the edge of the pavement structure; and
  • Providing gentle side slopes that are less prone to sliding.

These techniques, along with construction quality control, reduce the likelihood the pavement will crack and settle in times of drought, it says.

“Droughts are beyond MDOT’s control and unpreventable,” says Commissioner Mike Tagert, Northern Transportation District.

“Even though we can’t predict or stop a drought, we do take necessary, preventative measures to protect our highway system and keep the traveling public safe.”

“Unfortunately, we can’t control Mother Nature,” adds Hall.

“Our top priority is the safety of the traveling public in Mississippi. I’m proud of our maintenance crews and engineers for the commitment they have shown and continue to show to keeping our roads safe during this drought.

“Their efforts are protecting lives each and every day.”

   

Tagged categories: Asphalt; Coating Materials; Department of Transportation (DOT); Infrastructure; North America; Roads/Highways

Comment Join the Conversation:

Sign in to our community to add your comments.


 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us