What do you think is the biggest cause of coating failures?


Answers Votes
Faulty workmanship 51%
Ineffective quality control 33%
Bad specifications 13%
Defective coating materials 2%


Suggest a topic

   

Tagged categories: Coating failure

Comment from Frederick Stefano, (11/2/2010, 8:47 AM)

Faulty workmanship can be overcome by effective Quality control on the job site. May add cost but will also save money down the road.


Comment from Rudi Rennert, (11/3/2010, 10:16 AM)

Agreed, Humans can never be perfect and the only way to minimize risk is to put process in place to check and re-check workmanship.


Comment from kv g, (11/3/2010, 11:48 AM)

Improper surface preparation is the best answer, but it can be included in faulty workmanship.


Comment from Lance C Futcher, (11/3/2010, 9:12 PM)

In supplying house paints to the DIY market there are two major contributing factors to paint failing ... 1) the seller of the paint failing to give clear and concise information on how to apply the coating and 2) the customer not following that advice and taking shortcuts to save time or money in the short term.


Comment from Blu Alexander, (11/5/2010, 9:00 AM)

I agree with g. KV. Surface preparation is the biggest problem but that should also come under Bad Specifications and Ineffective QC.


Comment Join the Conversation:

Sign in to our community to add your comments.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us