What are the most effective procedures for protecting steel and adjacent concrete?


Selected Answers

From Tom Schwerdt of Texas Department of Transportation on May 5, 2015:
If we simply look at effectiveness, you select the most corrosion-resistant grade of stainless steel for your conditions and ensure it is properly heat-treated, pickled and passivated. Similarly, you select the most durable concrete mix design (low water:cement ratio, added fly ash, low reactivity aggregate, etc) and use large amounts of stainless steel rebar. Finish the concrete with something like a rubbed finish, only then following up with an extremely durable coating. Ensure that your overall design eliminates any area where salts and debris could collect, or water could puddle or infiltrate. Prevent the public from coming in contact with your structure. Several of these items add significant cost (though probably not the design portion - that's just being mindful while you design), but cost wasn't mentioned in the question.

From Warren Brand of Chicago Coatings Group on May 4, 2015:
This is a complex question, with many variables. If aesthetics are not important, I would lean towards coatings with elastomeric characteristics and overcoat both the steel and concrete. If aesthetics are important, I would consider a bond-breaker solution, overcoating both substrates. We've designed and used both successfully.

Please sign in to submit your answer this question    

Tagged categories: Asia Pacific; Carbon Steel; Concrete; EMEA (Europe, Middle East and Africa); Galvanized steel; Good Technical Practice; Latin America; North America; Stainless steel; Steel


Current PSF Question | Submit a PSF Question | Full PSF Archive

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us