Under what types of exterior atmospheric exposures (other than marine) is it necessary to test for soluble salts?


Selected Answers

From Stephen Bothello of Jotun UAE Ltd on February 4, 2016:
Exterior Atmospheric exposures defined by ISO 12944, Corrosivity Category C3, C4 and C5 Industrial. This is basically locations where corrosion rates range from medium to high, caused by increased rate of air pollution and the daily wet (humidity/ condensation) and dry cycles,  like, for example, gas transmission pipelines and above ground water storage tanks. Specifically, when durability of 15 years or more  is desired, salt tests are essential, though the frequency may be less than on steel intended for marine environments. It is to be noted that a lot of steel not intended for exposure in marine environments is, however, exposed to marine environments, due to transportation by sea from distant countries, many times unprotected. Steel stored at project or yard lay-down sites or open areas may also get exposed to high salt levels from dust or industrial emissions. Salt contamination from abrasives used for blasting is an added factor.

From Jim Johnson of CHLOR*RID International Inc. on February 1, 2016:
The most commonly encountered soluble salts, chloride, sulfate and nitrate, are found all across the country. They come not only from marine environments, but also from burning fossil fuels and using industrial chemicals.  Maps available from the National Atmospheric Deposition Program show that salt contamination occurs everywhere in the US. In every case I have seen, in over 25 years that I've worked in this industry, testing is ALWAYS less costly than a premature failure.

Please sign in to submit your answer this question    

Tagged categories: Asia Pacific; EMEA (Europe, Middle East and Africa); Environmental Controls; Exterior coatings; Exterior painting; Latin America; North America; Salt exposure; Soluble salts


Current PSF Question | Submit a PSF Question | Full PSF Archive

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us