Paint 44, Liquid-Applied Organic Polymeric Coatings and Linings for Concrete Structures in Municipal Wastewater Facilities, Performance-Based

All Standards | SSPC Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: August 05, 2013
Updated On: August 05, 2013
Editorial Change:
 
This new standard establishes minimum performance standards for coatings used over concrete in municipal wastewater facilities, based on categories of service environments and structures within the facility. The specifier identifies the structure to be coated, then determines the performance requirements for coatings for the structure’s service environment based on a table included in the standard. An example of language that could be used to specify coating requirements from the standard is included in the nonmandatory notes

(Back to all Standards)

 
   

Tagged categories: Concrete; Concrete coatings and treatments; Specification; SSPC; Wastewater Plants
 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us