Articles (23)


Building a Solid Foundation for Concrete Floor Coatings: A Guide to Inspection and Surface Preparation

from D+D In Depth, November 2016 ; by Steven Reinstadtler, Covestro LLC

An attractive, durable concrete floor coating requires methodical preparation before ...


Measuring Surface Profile on Bare Metal Surfaces Cleaned by Power Tools

from JPCL, August 2016


Measuring Surface Profile: What’s Changed, What’s the Same

from JPCL, July 2016


The Effect of Surface Preparation on Coating Performance

from JPCL, July 2016 ; by Patrick Cassidy, Elzly Technology Corporation and Paul Slebodnick, James Tagert and James Martin, U.S. Naval Research Lab

This article describes a study of the effect of profile type, profile height, the ext...


Development of Materials and Process Metrics for High-Performance Abrasive Blast Surface Preparation

from JPCL, February 2016 ; by Robert Kogler and Laura Erickson, Rampart LLC

The authors describe ongoing work being conducted with the Center for Corrosion Scien...


Replica Tape: Unlocking Hidden Information

from JPCL, July 2015 ; by David Beamish, DeFelsko Corporation

A surface profile is composed of a complex pattern of peaks and valleys. This article...


Running a Tight Ship: UHP Waterjetting and Surface-Tolerant Coatings in Newbuilding Applications

from JPCL, July 2015 ; by Nuno Cipriano, Ultrablast Lassarat Ltd., Brazil

This article describes how these combined technologies in newbuilding projects can pr...


Surfaces, Standards and Semantics: A Close Look at Surface Cleaning Standards: Hand- and Power-Tool Cleaning

from JPCL, May 2015 ; by Rob Francis, R A Francis Consulting Services Pty Ltd

Part 1 of this column on surface preparation standards, published in the February 201...


Roughing It Up

from D+D Print, January 2015 ; by Joe Reardon, SASE

When concrete needs profiling, these machines get it done.


On surface prep challenges, time & costs

from JPCL, December 2014

A specification for a bridge to be built of high-performance weathering steel requir...


Over-the-Top Performance

from D+D Print, November 2014 ; by Frank Lewis, SUNDEK Decorative Concrete Products

For decorative concrete overlays that perform, avoid these ‘wrong turns.’


SSPC's Latest Paint Application Standards Meet Field and Lab Needs

from JPCL, Three Decades of Change in the Coatings Industry 2013 Special Issue; by The JPCL Staff


Why surface preparation is important

from JPCL, May 2013 ; by Robert Barnhart, Debbie Mericle, Chuck Mobley, Tom Hocking, Jeff Bogran, and Ernestine McDaniel


New SSPC Standard Helps Determine Compliance with Profile Requirements

from JPCL, December 2012 ; by Aimée Beggs and Heather Stiner, SSPC: The Society for Protective Coatings

The authors report on a new standard, SSPC-PA 17, on steel profile and its complement...


Remedying excessive profile

from JPCL, September 2011

This Month's Question: What is the remedial action if a blaster produces too high a ...


Characterizing Surfaces after UHP Waterjetting in New Ship Construction

from JPCL, May 2011 ; by Philippe Le Calvé, DCNS, France; Jean-Pierre Pautasso, Direction Générale de I’Armement, France; and Nathalie Le Bozec, French Corrosion Institute

The authors report on the first part of a study on the use of UHP waterjetting for se...


Angels and Demons in the Realm of Protective Coatings: The Underworld of VOCs

from JPCL, April 2011 ; by Mike O’Donoghue, Ph.D.; V.J. Datta, MS; and Russell Spotten, International Paint, LLC

The authors examine the "angels and demons" that coatings with exempt solvents pose f...


Getting the right profile on weathering steel

from JPCL, June 2010


Problem Solving Forum: On measuring surface profile in the field

from JPCL, February 2010


How Does Waterjet Cleaning Affect the Surface and Surface Preparation?

from JPCL, January 2010 ; by Lydia M. Frenzel, Ph.D., Advisory Council

This article describes the history of waterjet cleaning, discusses the effect that pr...


An Overview of Preparing Concrete for Coatings: What to Ask, What to Do, and Where to Find Help

from JPCL, May 2009 ; by Fred Goodwin, Fellow Scientist, BASF Construction Chemicals

Key questions to ask about the surface preparation of concrete are covered in this ar...


Coating concrete: double-check your specs

from JPCL, May 2009 ; by Kevin Morris, Market Development Director, Water and Wastewater, The Sherwin-Williams Company

Editor's Note: This article is a condensed version of a paper the author presented at...


Problem Solving Forum: Controlling Surface Profile

from JPCL, March 2009

What are the causes of surface profile exceeding specified ranges, and how can surfac...


 
 
   

**Commercial white papers, product videos, and other sponsored documents posted on this site are paid content from third-party companies; inclusion and posting on this site does not imply an endorsement nor recommendation of the content by Technology Publishing/PaintSquare. By signing in and viewing or downloading this paid content, you agree to make your name and full contact information available to the sponsor of the content.

 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us