Coast Guard Cadets Analyze Corrosion Rates

A tank barge sank amid rough seas in Long Island Sound on Jan. 24, 1936, carrying 500,000 gallons of heating oil with it to the bottom of the sea.


New Coating Has Tie-Coat Properties

Hempel USA has introduced an anti-corrosive coating and primer with antifouling tie-coat properties for atmospheric and immersion service.


Coating Protects Immersion Equipment

A new epoxy coating offers high-temperature protection for oil and gas production equipment and other equipment operating under continuous immersion, Belzona announced.


see more news stories
 
 

Articles (9)


Bad Vibes: Using Coatings to Eliminate Vortex-Induced Vibration of Riser Strings on Deep-Water Offshore Structures

from JPCL, February 2016 ; by Peter Bock

When the length of the riser piping on an oil production platform increases for struc...


Protecting Offshore Wind Farm Towers

from JPCL, June 2015 ; by Hugues Dedeurwaerder, Coatings Research Institute

To ensure durability and corrosion protection in aggressive climates, the author disc...


see more articles
 
 

Video Learning Center (15)


Architectural Coatings: A PaintSquare Video Education Series

The D+D Pro Video Series: An archive of webinars hosted by DurabilityandDesign.com

A collection of archived webinars hosted by DurabilityandDesign.com focused on architectural coatings.


Concrete: A PaintSquare Video Education Series

The D+D Pro Video Series: An archive of webinars hosted by DurabilityandDesign.com

A collection of archived webinars hosted by DurabilityandDesign.com focused on concrete coatings and maintenance.


see more video learning center collections
 
 

Standards (1)


Standard Practice for Testing Water Resistance of Coatings Using Water Immersion

issued by ASTM

Immersion in water can cause the degradation of coatings. Knowledge on how a coating resists wa...


 
 
   

**Commercial white papers, product videos, and other sponsored documents posted on this site are paid content from third-party companies; inclusion and posting on this site does not imply an endorsement nor recommendation of the content by Technology Publishing/PaintSquare. By signing in and viewing or downloading this paid content, you agree to make your name and full contact information available to the sponsor of the content.

 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us