Report Details Cause of Foundation Cracks

New research confirms that pyrrhotite is to blame for premature cracking and deteriorating concrete foundations seen throughout hundreds of homes in Connecticut, but officials say important ...


Cracks Plague Sydney Metro Project

A multibillion-dollar metro rail extension in Australia’s largest city is facing a second major setback, as one of the precast concrete spans for the “Skytrain” rail bridge has cracked, the ...


Condo Builder, Subs Settle $36M Dispute

After six years of litigation, a large Southeastern U.S. builder and more than a dozen of its subcontractors have agreed to pay $22.5 million to settle a construction defect lawsuit involvin...


see more news stories
 
 

Blogs (2)


Steps to Assessing Concrete Structures

by Wiss, Janney, Elstner Associates Inc.

An assessment of a concrete structure to evaluate existing conditions and determine c...


‘I’m Simply Painting Some Concrete…’

by Burt Olhiser

Coating new concrete is a simple matter, correct? All you need to do is use a manufac...


 
 

Articles (11)


Basics of Corrosion in Reinforced Concrete

from JPCL, August 2015 ; by Fred Goodwin and Frank Apicella, BASF Construction Chemicals

Corrosion in reinforced concrete has been an issue since it was first introduced and ...


On filling voids in concrete

from JPCL, April 2015


see more articles
 
 

Video Learning Center (15)


Architectural Coatings: A PaintSquare Video Education Series

The D+D Pro Video Series: An archive of webinars hosted by DurabilityandDesign.com

A collection of archived webinars hosted by DurabilityandDesign.com focused on architectural coatings.


Concrete: A PaintSquare Video Education Series

The D+D Pro Video Series: An archive of webinars hosted by DurabilityandDesign.com

A collection of archived webinars hosted by DurabilityandDesign.com focused on concrete coatings and maintenance.


see more video learning center collections
 
 
   

**Commercial white papers, product videos, and other sponsored documents posted on this site are paid content from third-party companies; inclusion and posting on this site does not imply an endorsement nor recommendation of the content by Technology Publishing/PaintSquare. By signing in and viewing or downloading this paid content, you agree to make your name and full contact information available to the sponsor of the content.

 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us